350.4R-04: Design Considerations for Environmental Engineering Concrete Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 350.4R-04: Design Considerations for Environmental Engineering Concrete Structures

Author(s): ACI Committee 350

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 16

Keywords: buoyancy; clarifier; contraction; design; expansion; filler; flood; flotation; forces; hazardous; ice; impact; joint; load; overturning; reservoir; safety; sealant; sliding; stability; tank; tension; torque; vibration; waterstop; weights.

DOI:

Date: 2/27/2004

Abstract:
Environmental engineering concrete structures provide conveyance, storage, and treatment of water, wastewater, and other materials. This report outlines special design considerations such as loads, stability, joint details, and special design conditions that are unique to these types of structures as well as ancillary structures.