Paradigms in Concrete Design and Aesthetics

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Paradigms in Concrete Design and Aesthetics

Author(s): Moncef Nehdi and Andres Bernal

Publication: Concrete International

Volume: 26

Issue: 6

Appears on pages(s): 60-64

Keywords: Design, paradigm, aesthetics, color, shape

DOI:

Date: 6/1/2004

Abstract:
Design of concrete structures has traditionally been perceived as a problem-solving exercise whereby the designer tries to develop an economic and functional structure that satisfies a set of design code provisions and meets a client’s needs. This article advocates a paradigm shift for concrete design to rather become a problem-finding process in which the aesthetic, social and environmental value of a structure becomes a central part of its functional design. Concrete has a substantial aesthetic potential, being a versatile design medium that lends itself to boundless creative shapes and visual treatments.