Fabric-Formed Concrete Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Fabric-Formed Concrete Columns

Author(s): Mark West

Publication: Concrete International

Volume: 26

Issue: 6

Appears on pages(s): 42-45

Keywords: Fabric-Formed Concrete Columns

DOI:

Date: 6/1/2004

Abstract:
Casa Dent is a single story concrete structure with a flat-plate roof slab supported by 13 cast-in-place, fabric-formed, reinforced concrete columns. Fabric formwork was chosen for this project because of its unique architectural and sculptural capabilities. Beyond the architectural advantages offered by this method, however, there are several unique technical aspects to this project that are worthy of discussion.