Cost-Effective Slabs-on-Ground

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cost-Effective Slabs-on-Ground

Author(s): Gregory Scurto, David Scurto, Wayne W. Walker, and Jerry A. Holland

Publication: Concrete International

Volume: 26

Issue: 5

Appears on pages(s): 65-67

Keywords:

DOI:

Date: 5/1/2004

Abstract:
As steel prices soar, plate dowels provide one solution to the material shortage problem.