Landmark Series: Tentative Recommendations for Prestressed Concrete (cont. from March 2004)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Landmark Series: Tentative Recommendations for Prestressed Concrete (cont. from March 2004)

Author(s): ACI-ASCE Committee 323

Publication: Concrete International

Volume: 26

Issue: 4

Appears on pages(s): 45-55

Keywords:

DOI:

Date: 4/1/2004

Abstract:
A guide to design and construction of safe, serviceable, linear structural members prestressed with high strength steel. Emphasis is on flexural members - beams, girders, and slabs. Most of the recommendations are applicable to both buildings and bridges. Design chapter treats: loading; allowable stress; prestress loss; flexure and shear; bond and anchorage; composite construction; continuity; end blocks; fire resistance; and cover and spacing of prestressing steel. Concrete, grout, prestressing steel, anchorages, and splices are covered in the section on materials. Construction section includes: transportation, placing, and curing of concrete; forms, shoring and falsework; placement of prestressing steel and application of the prestressing force; grouting; and handling and erection.