Underwater Concrete Part 3: Construction Issues

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Underwater Concrete Part 3: Construction Issues

Author(s): Sam X. Yao and Ben C. Gerwick, Jr.

Publication: Concrete International

Volume: 26

Issue: 3

Appears on pages(s): 60-64

Keywords:

DOI:

Date: 3/1/2004

Abstract:
In many marine construction projects, underwater concreting is technically demanding, usually on the critical path of the project schedule, and involves complex construction logistics. The underwater concreting portion of the project is an area where competent design and sound planning can achieve a meaningful reduction in both risk and cost. This article will discuss some technical considerations in the production and delivery, placement and protection, and form pressure of underwater concrete.