408R-03: Bond and Development of Straight Reinforcing Bars in Tension

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 408R-03: Bond and Development of Straight Reinforcing Bars in Tension

Author(s): ACI Committee 408

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 49

Keywords: anchorage; bond; concrete; deformed reinforcement; development length; reinforced concrete; reinforcement; relative rib area; splice; stirrup; tie

DOI:

Date: 9/24/2003

Abstract:
The performance of reinforced concrete structures depends on adequate bond strength between concrete and reinforcing steel. This report describes bond and development of straight reinforcing bars under tensile load. Bond behavior and the factors affecting bond are discussed, including concrete cover and bar spacing, bar size, transverse reinforcement, bar geometry, concrete properties, steel stress and yield strength, bar surface condition, bar casting position, development and splice length, distance between spliced bars, and concrete consolidation. Descriptive equations and design provisions for development and splice strength are presented and compared using a large database of test results. The contents of the database are summarized, and a protocol for bond tests is presented. Test data and reliability analyses demonstrate that, for compressive strengths up to at least 16,000 psi (110 MPa), the contribution of concrete strength to bond is best represented by the compressive strength to the 1/4 power, while the contribution of concrete to the added bond strength provided by transverse reinforcement is best represented by compressive strength to a power between 3/4 and 1.0. The lower value is used in proposed design equations. These values are in contrast with the square root of compressive strength, which normally is used in both descriptive and design expressions. Provisions for bond in ACI 318-02 are shown to be unconservative in some instances; specifically, the 0.8 bar size factor for smaller bars should not be used and a f-factor for bond is needed to provide a consistent level of reliability against bond failure. Descriptive equations and design procedures developed by Committee 408 that provide improved levels of reliability, safety, and economy are presented. The ACI Committee 408 design procedures do not require the use of the 1.3 factor for Class B splices that is required by ACI 318.