A New Source of Pozzolanic Material

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A New Source of Pozzolanic Material

Author(s): Tarun R. Naik and Rudolf N. Kraus

Publication: Concrete International

Volume: 25

Issue: 12

Appears on pages(s): 55-62

Keywords: Wood ash; properties; microstructure; recycling; pozzolan

DOI:

Date: 12/1/2003

Abstract:
Wood ash is generated as a by-product of combustion. It is essential to develop beneficial uses of wood ash to meet the challenges associated with its disposal. This investigation was undertaken with a view to understand various physical, chemical, and, microstructural properties of wood ash derived from various sources in the USA and Canada; and, to determine its potential applications in cement-based construction materials.