Recommendations for the Use of Models in ACI 318

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Recommendations for the Use of Models in ACI 318

Author(s): ACI Committee 444

Publication: Structural Journal

Volume: 88

Issue: 6

Appears on pages(s): 738-742

Keywords: models; prototypes; reliability; standards; structural analysis; structural design; Design

DOI: 10.14359/1289

Date: 11/1/1992

Abstract:
This report reviews the use of models in various codes, in North America and other countries. Also reviewed is the state of the art on the topic. Based on this review, recommendations are made for ACI 318 to include models as a viable tool for design of structures. References are also cited.