Title: 437R-03: Strength Evaluation of Existing Concrete Buildings

Author(s): ACI Committee 437

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 28

Keywords: cracking; deflection; deformation; deterioration; gravity load; load; load test; reinforced concrete; strength; strength evaluation; test.

DOI:

Date: 8/14/2003

Abstract:

Note: A newer version of this document exists. This document was replaced by 437R-19.

The strength of existing concrete buildings and structures can be evaluated analytically or in conjunction with a load test. The recommendations in this report indicate when such an evaluation may be needed, establish criteria for selecting the evaluation method, and indicate the data and background information necessary for an evaluation. Methods of determining material properties used in the analytical and load tests investigation are described in detail. Analytical investigations should follow the principles of strength design outlined in ACI 318. Working stress analysis can supplement the analytical investigations by relating the actual state of stress in structural components to the observed conditions. Procedures for conducting static load tests and criteria indicated for deflection under load and recovery are recommended.