Use of ACM in Rehabilitation Projects in Egypt

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of ACM in Rehabilitation Projects in Egypt

Author(s): A. Abdelrahman, M. Mohamadien, S. Rizkalla, and G. Tadros

Publication: Symposium Paper

Volume: 215

Issue:

Appears on pages(s): 361-372

Keywords: application; beam; carbon; construction; design; rehabilitation; slab

DOI: 10.14359/12877

Date: 8/1/2003

Abstract:
Use of ACM in the form of FRP laminates in rehabilitation of concrete structures is the prime application of ACM in Egypt. FRP laminates are applied for strengthening reinforced concrete slabs or beams in flexure and shear as well as for confinement of reinforced concrete columns. This paper briefly introduces selected projects to demonstrate the current practice of FRP in Egypt. In the first application, carbon FRP (CFRP) laminates in the form of strips and sheets were applied to strengthen a public building suffering from differential settlement of the foundation. In a different application, CFRP laminates were used to upgrade a residential building to be used for commercial purpose. The paper summarizes the design aspects, construction details and recommendations for future application of ACM.