Field Applications of FRP Strengthening in Egypt

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Field Applications of FRP Strengthening in Egypt

Author(s): I. Mahfouz and T. Rizk

Publication: Symposium Paper

Volume: 215

Issue:

Appears on pages(s): 279-290

Keywords: fiber reinforced polymer (FRP); reinforced concrete; repair; strengthening

DOI: 10.14359/12871

Date: 8/1/2003

Abstract:
The objective of this paper is to present some of the real life applications of fiber reinforced polymers (FRP) in Egypt. The authors of the paper have recently used carbon fiber reinforced polymers (CFRP) with great success to repair several types of structures, which include hotels, administrative buildings, and historical structures. This paper will provide a brief summary of some of the projects repaired or strengthened using CFRP.