Time-Dependent Deflections of Prestressed Members: Rational and Approximate Methods

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Deflections of Prestressed Members: Rational and Approximate Methods

Author(s): Alex Aswad

Publication: Symposium Paper

Volume: 129

Issue:

Appears on pages(s): 101-114

Keywords: camber; creep properties; deflection; prestress loss; shrinkage; prestressed concrete; pretensioning; viscoelasticity; Design

DOI: 10.14359/1285

Date: 12/1/1991

Abstract:
The long-term camber prediction under sustained loads is an important part of the design of pretensioned flexural members. Critical members are noncomposite roofs and bridge members which have medium or large span-depth ratios or elements made of lightweight concrete. Currently the most common approximate design method is one that relies on empirical multipliers applied to initial cambers and deflections. When compared to a rational approach, substantial differences in prediction of long-term camber or deflection are noticed. The approximate method appears to overestimate the permanent sag or underestimate the camber. It also does not consider certain creep, shrinkage, and relaxation properties. It is concluded that such methods may be unreliable for critical members and that the rational method is preferred. For preliminary design of longer spans, revised multipliers are suggested for use with the approximate method.