Abstract:
This article is presented, not through the eyes of a scientist, but rather through those of a practitioner in the industry. Experts say that concrete strength must reach 500 psi (4 MPa) to resist one freezing and thawing cycle. I feel that the key is having the right circumstances, the right non-chloride accelerator, and above all, the right team.