Maturity Method Speeds Form Cycling

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Maturity Method Speeds Form Cycling

Author(s): Michael Fox

Publication: Concrete International

Volume: 25

Issue: 10

Appears on pages(s): 92-94

Keywords:

DOI:

Date: 10/1/2003

Abstract:
On the Maricopa County 4th Avenue Jail project, the project manager did not have to wait for 7-day lab results to strip forms and reshores. Thanks to real-time, in-place concrete strength data from the intelliRock™ system, they saved time and money by renting less formwork and cycling it faster.