Hydraulic Concrete Placer Keeps Airport Project Flying Right

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Hydraulic Concrete Placer Keeps Airport Project Flying Right

Author(s): Kim Lacina

Publication: Concrete International

Volume: 25

Issue: 10

Appears on pages(s): 85-87

Keywords:

DOI:

Date: 10/1/2003

Abstract:
As part of a master plan to ease airport traffic congestion and further develop the Ft. Lauderdale-Hollywood International Airport, the construction of a multilevel, 9000-parking space, consolidated rental car facility (CRCF) is underway. When complete, the $180 million structure will provide public parking and house all of the airport’s rental car agencies. The new facility will simplify rental car pick-up and delivery, ease access to terminals, and eliminate the fleets of shuttle buses contributing to increased airport traffic. The CRCF will be 9 levels, 4.5 million ft2 (420,000 m2), and use 140,000 yd3 (110,000 m3) of concrete.