Abstract:
Picture, if you will, a concrete truck cruising down the highway, loaded with nine cubic yards of the latest high-tech materials. Now think about what you really see. Concrete? Your new floor slab being delivered? What a trained eye sees is four shrinkage cracks, a little curling, some crazing, and future maintenance costs.