Historic Restoration at CCNY Intricate, Ongoing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Historic Restoration at CCNY Intricate, Ongoing

Author(s): Michael Chusid

Publication: Concrete International

Volume: 25

Issue: 8

Appears on pages(s): 74-76

Keywords:

DOI:

Date: 8/1/2003

Abstract:
More than 40,000 pieces of ornamental precast concrete are being used to restore historic Shepard Hall at the City College of New York. A “thin shell” reconstruction approach allows replacement of the original failed cladding and terra cotta with conventional masonry and a new ornamental cladding. Use of a high-reactivity metakaolin to improve the strength and durability of the portland concrete mixtures is written into the project specifications.