Long-Term Durability of Sulphur Concrete in Harsh Chemical Environments

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Long-Term Durability of Sulphur Concrete in Harsh Chemical Environments

Author(s): G. J. Fallis

Publication: Symposium Paper

Volume: 214

Issue:

Appears on pages(s): 181-192

Keywords: chemical resistance; concrete repair; corrosion-proof; restoration; sulphur concrete

DOI: 10.14359/12771

Date: 6/17/2003

Abstract:
In recent years, sulphur concrete has proven to be capable of withstanding attack by some of the most aggressive chemicals used in industry. This fast setting, acid and salt resistant concrete is well suited for use in the mineral processing and fertilizer production industries. This paper briefly describes the properties, production, application and performance of this new construction material, with references to actual commercial installations and reviews the long term durability of these projects in harsh chemical environments.