Study on Performance of Concrete Using Ecocement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Study on Performance of Concrete Using Ecocement

Author(s): S. Tanaka, T. Nakamura, S. Meiarashi, and H. Kawano

Publication: Symposium Paper

Volume: 212

Issue:

Appears on pages(s): 1073-1092

Keywords: concrete; durability; ecocement; incinerator ash; leaching; strength

DOI: 10.14359/12739

Date: 6/1/2003

Abstract:
It was investigated whether normal ecocement manufactured using as raw materials large amounts of urban wastes such as incinerator ash and sewage sludge, could he used for reinforced concrete. It was confirmed that the fresh properties, strength properties, durability, steel corrosion protecting performance, leaching of heavy metals and workability of the concrete using normal ecocement that contains a reduced amount of chloride ions of around 0.05% were equal to those of concrete using normal portland cement. The results of test executions in several field also confirmed that concrete using ecocement demonstrated Workability equal to that of general concrete. Based on these results, it was concluded that normal ecocement can he used for reinforced concrete.