Sacrificail Cahodic Protection of RC-Structures Using a Zinc-Hydrogel Anode-Investigations on the Effectiveness

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sacrificail Cahodic Protection of RC-Structures Using a Zinc-Hydrogel Anode-Investigations on the Effectiveness

Author(s): M. Raupach and M. Bruns

Publication: Symposium Paper

Volume: 212

Issue:

Appears on pages(s): 127-142

Keywords: cathodic protection; reinforcement corrosion; sacrificial anode; zinc-hydrogel

DOI: 10.14359/12682

Date: 6/1/2003

Abstract:
Cathodic protection is used world-wide to protect reinforced concrete structures against reinforcement corrosion. Cathodic protection systems can generally be divided into impressed current systems and systems working with sacrificial anodes. The Zinc-Hydrogel Anode is one of these sacrificail anode systems. This paper presents investigation on the effectiveness of the Zinc-Hydrogel Anode to control rinforcement corrosion. The aim of this investigation was to find out how parameters like reinforcement content and position of the anode are affecting the effectiveness. As a result it was found, that the protection current density and the polarisation of the reinforcement are highly affected by both parameters.