Load Relaxation Tests on Heavy Duty Sleeve and Lead Caulking Expansion Anchors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Load Relaxation Tests on Heavy Duty Sleeve and Lead Caulking Expansion Anchors

Author(s): G. Senkiw

Publication: Symposium Paper

Volume: 130

Issue:

Appears on pages(s): 47-60

Keywords: anchors (fasteners); load tests; tension tests; Structural Research

DOI: 10.14359/1267

Date: 1/1/1992

Abstract:
Ninety-day load-relaxation tests at room temperature were conducted on a full range of sizes of heavy duty sleeve and lead caulking expansion anchors. The test results showed that the sleeve and lead caulking anchors on the average are able to retain only 60 and 40 percent of their initial tension load, respectively.




  