Ductility Enhancement of Moderately Confined Concrete Tied Columns with Hook-Clips

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductility Enhancement of Moderately Confined Concrete Tied Columns with Hook-Clips

Author(s): Panitan Lukkunaprasit and Chadchart Sittipunt

Publication: Structural Journal

Volume: 100

Issue: 4

Appears on pages(s): 422-429

Keywords: ductility; hook; reinforced concrete.

DOI: 10.14359/12650

Date: 7/1/2003

Abstract:
An experimental investigation of the effectiveness of hook-clips in improving the performance of conventional 90-degree hook-ties and crossties in moderately confined reinforced concrete (RC) tied columns is described. The tie configurations provided in the five large-scale specimens tested included 90-degree hook-ties and crossties, with and without hook-clips, and 135-degree hook-ties. The columns were subjected to moderate levels of compression and cyclic lateral loads. The hook-clips were found to be effective in improving the performance of concrete columns confined with 90-degree hook-ties and crossties, resulting in the displacement ductility factor and energy dissipation capacity to be increased by approximately 85 and 400%, respectively.