Crack Width Prediction Using Compatibility-Aided Strut-and-Tie Model

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Crack Width Prediction Using Compatibility-Aided Strut-and-Tie Model

Author(s): Ronnie R. H. Zhu, Wirat Wanichakorn, Thomas T. C. Hsu, and John Vogel

Publication: Structural Journal

Volume: 100

Issue: 4

Appears on pages(s): 413-421

Keywords: bent caps; cracking; reinforced concrete.

DOI: 10.14359/12649

Date: 7/1/2003

Abstract:
Unacceptable diagonal cracks frequently occur at service load in the vicinity of the re-entrant corners in structures such as the dapped ends of bridge girders and the ledges of inverted T bent caps. Such diagonal cracks are not only visually intimidating but also impose a potential danger of corrosion of reinforcing bars. Controlling such cracking is difficult due to the lack of a rational theory for crack prediction. In this paper, a compatibility-aided strut-and-tie model (CASTM) is proposed for predicting the diagonal crack widths at re-entrant corners. The validity of this model is supported by tests of seven full-scale specimens.