330.1-03: Specification for Unreinforced Concrete Parking Lots

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 330.1-03: Specification for Unreinforced Concrete Parking Lots

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 6

Keywords: concrete parking lots; concrete pavements; construction; curing; inspection testing; jointing; pavement; specifications; texturing

DOI:

Date: 3/24/2003

Abstract:

Note: A newer version of this document exists. This document was replaced by 330.1-14.

Note: 330.1-03 is only available in PDF format.

This specification covers minimum requirements for the construction of unreinforced concrete parking lots on grade. Included are requirements for materials, placing, texturing, curing, jointing, and opening to traffic.