Evaluation of Effect of August 17, 1999, Marmara Earthquake on Two Tall Reinforced Concrete Chimneys

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of Effect of August 17, 1999, Marmara Earthquake on Two Tall Reinforced Concrete Chimneys

Author(s): Sami A. Kilic and Mete A. Sozen

Publication: Structural Journal

Volume: 100

Issue: 3

Appears on pages(s): 357-364

Keywords: bond; flexural strength; reinforced concrete; shear; splice

DOI: 10.14359/12611

Date: 5/1/2003

Abstract:
Two tall reinforced concrete chimneys, Stacks 25F-5 (115 m) and 36F-5 (107.5 m), were subjected to strong ground motion during the August 17, 1999, Marmara earthquake. Stack 25F-5 failed while Stack 36F-5 survived. Both stacks were designed in accordance with ACI 307-69. This study reports the earthquake parameters, the ground motion measured within 3 km of the stacks, and the structural properties of the stacks. Evaluation of the response bounds of the stacks leads to the conclusion that the region of flexural yielding remained at the base of Stack 36F-5 while it was at a level approximately 35 m above base for Stack 25F-5 because it had a large penetration extending from 30 to 35 m. The collapse of Stack 25F-5 was not due to lack of strength caused by design or material deficiencies but was due to the presence of reinforcing-bar splices in the region where flexural yielding occurred.