Cyclic Loading of Ductile Precast Concrete Beam-Column Connection

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cyclic Loading of Ductile Precast Concrete Beam-Column Connection

Author(s): Ali R. Khaloo and H. Parastesh

Publication: Structural Journal

Volume: 100

Issue: 3

Appears on pages(s): 291-296

Keywords: beam-column; joint; load; moment; precast

DOI: 10.14359/12603

Date: 5/1/2003

Abstract:
In this study, a simple moment-resisting precast concrete beam-column connection is proposed for highly seismic regions. An experimental study was carried out to investigate the connection behavior subjected to cyclic inelastic loading. Four precast beam-column interior connections and one monolithic connection were tested. The variables examined were the connection length of reinforcements and presence of transverse bars at mid-height of connection. The specimens were tested with the column under a constant axial compressive load and reverse cyclic loading in accordance with a prescribed displacement history. Connection performance is evaluated on the basis of ductility, energy dissipation capacity, connection strength, and drift capacity. Based on test results, the precast connection is capable of matching or exceeding the performance of the monolithic connection and thereby provides moment-resisting behavior.


ALSO AVAILABLE IN:

Electronic Structural Journal