Experimental Evaluation of ACI and AASHTO-LRFD Design Provisions for Combined Shear and Torsion

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Evaluation of ACI and AASHTO-LRFD Design Provisions for Combined Shear and Torsion

Author(s): Khaldoun N. Rahal and Michael P. Collins

Publication: Structural Journal

Volume: 100

Issue: 3

Appears on pages(s): 277-282

Keywords: beam; bridge; reinforced concrete; shear; strength; torsion

DOI: 10.14359/12601

Date: 5/1/2003

Abstract:
The experimental results from four large nonprestressed specimens loaded in combined shear and torsion are used to evaluate the torsion design procedures of ACI 318-02 and AASHTO-LRFD. Both sets of procedures calculate the required amounts of hoop reinforcement for torsion based on a space truss model with compression diagonals inclined at an angle of q to the longitudinal axis. It is shown that the ACI provisions give very conservative results if the recommended value of 45 degrees is used for q. If the lower limit of 30 degrees is used, however, some unconservative results are possible. The AASHTO-LRFD provisions predicted values of q of approximately 36 degrees for these specimens and gave accurate estimates of the strengths.