Seismic Safety Assessment of Reinforced Concrete Frame-Wall Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Safety Assessment of Reinforced Concrete Frame-Wall Buildings

Author(s): Zekai Akbay and Haluk M. Aktan

Publication: Structural Journal

Volume: 88

Issue: 6

Appears on pages(s): 693-700

Keywords: axial loads; bending moments; buildings; reinforced concrete; earthquake-resistant structures; safety; shear properties; shear strength; shear stress; walls; Structural Research

DOI: 10.14359/1260

Date: 11/1/1992

Abstract:
A method to evaluate the vulnerability of reinforced concrete structural walls to shear failure is presented. The method utilizes an experimentally developed shear stiffness model for distribution of shear stresses along reinforced concrete structural walls. Seven wall specimens tested by other investigators are analyzed to assess their shear strength supply and critical moment-to-shear ratios. The predicted shear strengths provide lower bounds to actual measured strengths.