Seismic Behavior of Eccentric R/C Beam-Column-Slab Connections Under Sequential Loading in Two Principal Directions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Eccentric R/C Beam-Column-Slab Connections Under Sequential Loading in Two Principal Directions

Author(s): B. Burak and J. K. Wight

Publication: Symposium Paper

Volume: 209

Issue:

Appears on pages(s): 863-880

Keywords: beam-to-column connections; eccentricity; joint shear distortion; loading in two principal directions; seismic behavior

DOI: 10.14359/12536

Date: 9/26/2002

Abstract:
The performance of beam-to-column connections subjected to reversed cyclic loading depends on several variables. In this investigation, the effects of eccentric spandrel beams, wide normal beams, column section aspect ratio, loading in two principal directions, and slab participation on the inelastic behavior of beam-to-column connections are studied. The experimental program features three 3/4-scale exterior reinforced concrete beam-column-slab subassemblies. The major design variables for the specimens are the eccentricity of the spandrel beam with respect to column, beam and column section aspect ratios, and joint shear stress level. Results of the experimental program, including load-displacement response, beam plastic hinge rotation, joint distortion, and bond deterioration are presented in this paper.