Guidelines for the Design of Post-Tensioned Floors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guidelines for the Design of Post-Tensioned Floors

Author(s): Bijan O. Aalami and Jennifer D. Jurgens

Publication: Concrete International

Volume: 25

Issue: 3

Appears on pages(s): 77-83

Keywords:

DOI:

Date: 3/1/2003

Abstract:
This article presents a set of guidelines intended to assist designers in routine post-tensioning design, beginning with a discussion of the initial decisions that must be made to design post-tensioned floor members. We then provide a set of recommendations, derived from industry practice, which have yielded economical designs with good in-service performance. Where applicable, we based the guidelines on ACI 318-02 and IBC 2000.