Seismic Behavior of Reinforced Concrete Braced Frame

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Behavior of Reinforced Concrete Braced Frame

Author(s): Shan-Hua Xu and Di-Tao Niu

Publication: Structural Journal

Volume: 100

Issue: 1

Appears on pages(s): 120-125

Keywords: brace; ductility; load; reinforced concrete; seismic; stiffness.

DOI: 10.14359/12446

Date: 1/1/2003

Abstract:
The results of an experimental program in which seven reinforced concrete (RC) braced frames with different bracing, one reinforced concrete frame, and one reinforced concrete shear wall were tested under vertical loading and reversed cyclic horizontal loading are described in this paper. The research focused mainly on the failure mechanism, strength, degradation in stiffness, and hysteresis loop of the reinforced concrete braced frame.