N-M-V Interaction Domains for Box and I-Shaped Reinforced Concrete Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: N-M-V Interaction Domains for Box and I-Shaped Reinforced Concrete Members

Author(s): Antonino Recupero, Antonino D’Aveni, and Aurelio Ghersi

Publication: Structural Journal

Volume: 100

Issue: 1

Appears on pages(s): 113-119

Keywords: flexural strength; reinforced concrete; shear strength; steel.

DOI: 10.14359/12445

Date: 1/1/2003

Abstract:
This paper proposes an approximate physical model to evaluate the N-M-V interaction resistance domains for box and I-shaped concrete cross sections. The model subdivides the concrete beam in layers, with nearly constant stress fields, and determines the internal forces satisfying equilibrium of the cross section, applying the static theorem of plasticity (lower bound theorem). The resisting contribution of the web longitudinal reinforcements is also considered by including stress fields of variable inclination on the longitudinal element direction. The proposed model leads to a conservative evaluation of bearing capacity and permits to numerically obtain the N-M-V interaction resistance domains of the indicated cross sections. The obtained N-M-V failure surfaces are in good agreement with the experimental evidences of tests performed by P. Regan and H. Rezai-Jorabi and by J. R. Robinson and J. M. Demorieux.