Carbonation and Chloride-Induced Corrosion of Reinforcement in Fly Ash Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Carbonation and Chloride-Induced Corrosion of Reinforcement in Fly Ash Concrete

Author(s): M. N. Haque and M. Kawamura

Publication: Materials Journal

Volume: 89

Issue: 1

Appears on pages(s): 41-48

Keywords: calcium chlorides; carbonation; compressive strength; concretes; corrosion; fly ash; fresh concretes; half-cell potential; Materials Research

DOI: 10.14359/1243

Date: 1/1/1993

Abstract:
Two grades of concretes with and without fly ash and with and without CaCl 2, with total cementitious contents of 250 and 350 kg/ 3, were designed. The concretes were cast with 0, 0.5, and 2 percent of Cl - by weight of cementitious materials. The compressive strength development, extent of carbonation, and the half-cell potential of steel bars in the various concrete specimens exposed to the outdoors were monitored for a period of up to 4 years. The results of this investigation indicate that concretes with 30 percent replacement of cement by fly ash, on equal weight basis, carbonated more than the control concretes. The 4-year strength of the fly ash concretes, however, was 18 percent less than the plain concretes. The results also suggest that the half-cell potential referenced to CSE is not a reliable indicator of the extent of corrosion. The extensive cracking in all the reinforced fly ash concrete specimens with 2 percent Cl - of the total cementitious content establishes the comparatively higher corrosion susceptibility of concretes made with fly ash.


ALSO AVAILABLE IN:

Electronic Materials Journal