Alternative design for the non-slender beam (deep beam)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Alternative design for the non-slender beam (deep beam)

Author(s): Tjen N. Tjhin and Daniel A. Kuchma

Publication: Symposium Paper

Volume: 208

Issue:

Appears on pages(s): 81-90

Keywords:

DOI: 10.14359/12413

Date: 10/29/2002

Abstract:
A 20 ft (6.10 m) span deep beam was designed using the strut-and-tie method according to ACI 318-02 Appendix A. The beam is 20 in. (508 mm) wide and 80 in. (2032 mm) deep and carries two concentrated factored loads, V, of 360 kips (1601 kN) each. Bearing plates of 18 in. x 20 in. (457 mm x 508 mm) are provided at all loading and support locations. The self-weight was not considered in the design. The compressive strength of concrete, fc and the yield strength of the steel reinforcement, fy are taken as 4 ksi (27.6 MPa) and 60 ksi (414 MPa), respectively. A simple strut-and-tie model shown in Fig. (1 b-2) is used in the design. The provided reinforcement for the main tie is 2 layers of 5 #9 (#29 mm) bars. The anchorages of these bars are provided by means of standard 90’ hooks. The reinforcement details are shown in Fig. (1 b-6).