Comparison Beween Accelerated and Natural Carbonation Results in Different Concretes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparison Beween Accelerated and Natural Carbonation Results in Different Concretes

Author(s): M.A. Sanjuan, C. Andrade, and M. Cheyrezy

Publication: Symposium Paper

Volume: 207

Issue:

Appears on pages(s): 263-278

Keywords: carbonation; concrete; durability; fly ash; silica fume; testing methods

DOI: 10.14359/12395

Date: 10/7/2002

Abstract:
Carbonation is one of the main contributors to reinforcement corrosion. The testing of concrete carbonation is usually done by introducing the specimens in chambers of different CO2 concentrations. The present paper describes ,an evaluation of the effectiveness of accelerated carbonation testing as a mean of prediction of the natural process of carbonation of concrete. The concrete samples were submitted to natural (0,03% COz) and accelerated. (5% or 100% COz) carbonation. The results are compared by calculating the diffusion coefficients and the depth of carbonation. They shotw that accelerated carbonation of concrete changes with respect to that found in natural conditions when supplementary cementing materials are present.