Properties of Super Low-Heat Cement Incorporating Large Amounts of Ground Granulated Blast Furnace Slag of High Fineness

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Super Low-Heat Cement Incorporating Large Amounts of Ground Granulated Blast Furnace Slag of High Fineness

Author(s): T. Tomisawa, T. Chikada, and Y. Nagao

Publication: Symposium Paper

Volume: 132

Issue:

Appears on pages(s): 1385-1400

Keywords: adiabatic conditions; blast furnace slag; bleeding (concrete); carbonation; compressive strength; drying shrinkage; heat of hydration; fineness; low-heat cements; temperature; Materials Research

DOI: 10.14359/1233

Date: 5/1/1992

Abstract:
Recently in Japan, super low-heat cement (SLHC) with a much lower heat of hydration than the moderate heat portland cement generally used in massive concrete structures has been demanded for reducing the thermal cracking of mass concrete. To satisfy the requirement, the SLHC (heat of hydration: 167 kJ/kg at 28 days; compressive strength: 30 MPa at 28 days, complying with Japanese industrial standards), incorporating Blaine fineness > 600 m¦/kg and a large amount of ground granulated blast furnace slag (GGBS), has been developed. The effects of fineness and content of GGBS on heat of hydration and compressive strength of cement are described. Included also are test results of the bleeding ratio, compressive strength, adiabatic temperature rise, drying shrinkage, and carbonation depth of concrete using the SLHC.