Influence of Slag Type and Replacement Level on Strength Elasticity, Shrinkage and Creep of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Slag Type and Replacement Level on Strength Elasticity, Shrinkage and Creep of Concrete

Author(s): J. J. Brooks, P. J. Wainwright, and M. Boukendakji

Publication: Symposium Paper

Volume: 132

Issue:

Appears on pages(s): 1325-1342

Keywords: blast furnace slag; blended cements; creep; slag cements; slags; modulus of elasticity; shrinkage; strength; Materials Research

DOI: 10.14359/1230

Date: 5/1/1992

Abstract:
Ten blended slag-cement concretes made with typical slags from four countries are compared with a control ordinary portland cement concrete. The slags replaced 30 to 70 percent of cement by mass. Concretes are compared on the basis of equal mass proportions of cementitious materials, aggregates, and water. Average strength, elasticity, and creep are quantified relative to the corresponding properties of the control concrete. The influence of type of slag on concrete properties is inconsistent and small. The influence of replacement level on strength and creep is time-dependent. For water-stored mature concrete, slag enhances the secant modulus of elasticity, but the opposite occurs for dry-stored concrete. Compared with OPC concrete, slag-cement concrete has a similar or greater long-term strength, similar shrinkage, lower basic creep, and similar or lower total creep.