Textile Fabrics for Cement Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Textile Fabrics for Cement Composites

Author(s): A. Pelad and a. Bentur

Publication: Symposium Paper

Volume: 206

Issue:

Appears on pages(s): 341-354

Keywords: bond, cement, composite, fabric, fiber, flexure, pull-out, yarn

DOI: 10.14359/12262

Date: 4/1/2002

Abstract:
One of the most efficient ways to obtain a high performance cementitious composite is by reinforcement with continuous fibers. Production of such composites can be accomplished by the use of textile fabrics, which are impregnated with cement paste or mortar. The present paper provides and overview of the major characteristics in predicting the performance of cement (weft insertion warp knit, short weft warp knit and woven fabrics) as well as found that the geometry of a given fabric could enhance the bonding and enable one to obtain strain hardening behavior with low modulus yarn fabrics. On the other hand, variations of the geometry in a fabric could drastically reduce the efficiencey, resulting in a rduced strengtheniong effect of the yarns in the fabric relative to single yarns not in a fabric form. The improved bonding in low modulus yarn was found to be mainly the result of the special shape of the yarn induced by the fabric. Therefore, in cement composites, the fabrics cannot be viewed simply as a means for holding together continuous yarns so that they can be readily placed in the matrix.