Modeling of Restrained Shrinkage Cracking in Concrete Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling of Restrained Shrinkage Cracking in Concrete Materials

Author(s): S. A. Mane, T. K. Desai, D. Kingsbury, and B. Mobasher

Publication: Symposium Paper

Volume: 206

Issue:

Appears on pages(s): 219-242

Keywords: cementitious composites, cracking, creep, fibers, restrained shrinkage

DOI: 10.14359/12255

Date: 4/1/2002

Abstract:
An experimental study was conducted to evaluate the restrained shrinkage cracking in plain and fiber reinforced concrete. The experiment utilizes a constant humidity chamber holding the restrained shrinkage specimens. The chamber is subjected to constant flow of air around the specimens. The strain in the restraining steel and the crack width in the concrete samples were monitored continuously. The experimentally obtrained results are affected by geometry of the specimen, the humididty and shrinkage conditions, and the restraing offered by stiffness of the steel ring. In addition, concrete properties such as the stiffness, shrinkage and creep affect the response. In order to better understand the restrained shrinkage of concrete under the proposed test method and eliminate the influence of test conditions, an analytical approach was developed. The model incorporates key influential parameters of shrinkage, creep, aging, and microcracking, in the stress analysis of a restrained concrete section. The theoretical model was used to calibrate and interpret the experimental test results.