Air-Void Stability in Self-Consolidating Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Air-Void Stability in Self-Consolidating Concrete

Author(s): Kamal H. Khayat and Joseph Assaad

Publication: Materials Journal

Volume: 99

Issue: 4

Appears on pages(s): 408-416

Keywords: admixture; air void; consolidation

DOI: 10.14359/12224

Date: 7/1/2002

Abstract:
Ensuring an adequate and stable air-void system in flowable concrete is essential to guarantee proper resistance to freezing and thawing. Ten self-consolidating concrete (SCC) mixtures were prepared to evaluate the influence of mixture proportioning on the stability of the air-void system during agitation. Samples were taken at different time intervals over a period of 95 min after the initial water-cement contact to analyze the air-void system and determine its variation with agitation. Bingham rheological parameters (plastic viscosity and yield stress), slump flow, filling capacity, V-funnel flow time, and surface settlement were evaluated. The modified point-count method was employed to determine the characteristics of the corresponding air-void system. Test results show that the air-void characteristics of SCC can be similar to those found for normal-slump concrete. In general, greater air-void stability can be obtained when the SCC is proportioned with a higher content of cementitious materials and a lower water-cementitious materials ratio (w/cm). For mixtures with a relatively low content of cementitious materials and a high w/cm, the air-void stability increases when a viscosity-modifying admixture is incorporated. To prevent coalescence of small air bubbles during agitation, the plastic viscosity and yield stress values should not exceed 10 N.m.s and 2 N.m, respectively. Such limits are also shown to yield greater air-void stability after 95 min of occasional agitation.


ALSO AVAILABLE IN:

Electronic Materials Journal