Repairing Concrete Hydraulic Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Repairing Concrete Hydraulic Structures

Author(s): Claude Gliddon

Publication: Journal Proceedings

Volume: 44

Issue: 3

Appears on pages(s): 513-518

Keywords: none

DOI: 10.14359/12189

Date: 3/1/1948

Abstract:
Seventeen years experience of the Gatineau Power Co. indicate that ordinary concrete, reinforced and unreinforced, can be successfully used to repair hydraulic structures. Elimination of leakage prior to surface repair, good bond between new and old concrete, and shrinkage of new concrete during setting to prevent cracking are important. A porcedure for repair is outlined stressing the importance of experienced labor and supervision and briefly describing grouting, selection of materials, design strengths of concrete, preparatin of surface, vibration, forms, curing and joints.