Title: Monolithic and Bonded Floor Finishes

Author(s): Morgan B. Klock

Publication: Journal Proceedings

Volume: 45

Issue: 6

Appears on pages(s): 725-730

Keywords: no keywords

DOI: 10.14359/12182

Date: 6/1/1949

Abstract:
The author discusses the design and construction of two types of floor finish. A floor capable of withstanding heavy wear, either bonded or monolithic finish, can be obtained by using a stiff mix of sound, well-graded materials which is throughly compacted with a power float. Hard coarse and fine aggregates are recommended for the greatest resistance to wear.