Control of Quality of Ready-Mixed Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Control of Quality of Ready-Mixed Concrete

Author(s): Stanton Walker

Publication: Journal Proceedings

Volume: 45

Issue: 4

Appears on pages(s): 569-578

Keywords: no keywords

DOI: 10.14359/12171

Date: 4/1/1949

Abstract:
Control of quality of ready-mixed concrete is discussed. The objective of this paper is to pose the more important problems of concrete control, espically those peculiar to ready-mixed concrete, with the view of elicting discussion, rather than to attempt to outline recommended practices. Both central mixing and transit-mixing are discussed. Attention is directed to the mutuality of responsiblities of the producers and users in brining about effective control.