Concrete of the Future

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete of the Future

Author(s): Robert F. Blanks

Publication: Journal Proceedings

Volume: 45

Issue: 4

Appears on pages(s): 565-568

Keywords: no keywords

DOI: 10.14359/12170

Date: 4/1/1949

Abstract:
Mr. Blanks, in his remarks as retiring president, depicts what concrete miht be in 50 years in the future and discusses the role of the engineer in that era.