Title: Construction Practices for Architectural Concrete

Author(s): E. B. Oberly

Publication: Journal Proceedings

Volume: 45

Issue: 3

Appears on pages(s): 541-552

Keywords: no keywords

DOI: 10.14359/12169

Date: 3/1/1949

Abstract:
Detailed plans and carefully drawn specifications executed by a contractor and superintendent with the know-how of form construction are necessary for good architectural concrete. This paper describes some of the more important construction practices to be considered to achieve the results desired. Form details and concrete quality are discussed in considerable detail, the former being supported by illustrations.