Early Age Temperature Effects on Concrete Strength Prediction by the Maturity Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Early Age Temperature Effects on Concrete Strength Prediction by the Maturity Method

Author(s): Nicholas J. Carino, H. S. Lew, and Charles K. Volz

Publication: Journal Proceedings

Volume: 80

Issue: 2

Appears on pages(s): 93-101

Keywords: age-strength relation; compressive strength; concretes; curing; cylin-ders; temperature; tests.

DOI: 10.14359/12166

Date: 3/1/1983

Abstract:
A comparison was made between the strength-maturity relations of concrete cylinders cured outdoors and cylinders cured in a laboratory. It was found that when early age (assumed as 48 hr) temperatures of the outdoor-cured and laboratory-cured cylinders were similar, the strength-maturity relations were similar despite temperature fluctua-tions experienced by the outdoor-cured specimens. The relations were dissimilar when their early age temperatures differed. Another series of testsfurther investigated and confirmed the importance of early age temperature on the strength-maturity relation.