Use of Prepacked Aggregate Concrete in Major Dam Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Prepacked Aggregate Concrete in Major Dam Construction

Author(s): Paul Baumann

Publication: Journal Proceedings

Volume: 45

Issue: 11

Appears on pages(s): 229-235

Keywords: no keywords

DOI: 10.14359/12143

Date: 11/1/1948

Abstract:
This paper sets forth the method of construction of a major gravity dam whereby the average temperature of the mass concrete may be controlled within the mean annual and the dry shrinkage reduced to a fraction of that of conventional concrete by means of prepackaging of the coarse aggregate to a density corresponding to 30 percent voids; precooling the aggregate; the intrucsion of the coarse aggregate by mortar with a cement content of two sacks per cu yd or less; and the internal post-cooling, curing and draining of the mass concrete. (This process is known as the Prepakt method of construction.)