Title: High-Performance High-Volume Fly Ash Concrete

Author(s): V.M. Malhotra

Publication: Concrete International

Volume: 24

Issue: 7

Appears on pages(s): 30-34

Keywords:

DOI:

Date: 7/1/2002

Abstract:
In recent years, an emerging technology known as high-performance high-volume fly ash (HVFA) concrete has become available, which incorporates large volumes of fly ash into conventional portland cement concrete. This article outlines the fundamentals of high-performance HVFA concrete, gives its properties and durability characteristics, and makes a case for applicability use in the construction of highways in developing countries like China and India. . .




  