Cracking in Reinforced Concrete Bent Caps

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Cracking in Reinforced Concrete Bent Caps

Author(s): Bradley S. Young, Joseph M. Bracci, Peter B. Keating, and Mary Beth D. Hueste

Publication: Structural Journal

Volume: 99

Issue: 4

Appears on pages(s): 488-498

Keywords: beam; cap; cracking; reinforcement; shear

DOI: 10.14359/12118

Date: 7/1/2002

Abstract:
This paper presents the findings from an experimental investigation into the causes of unexpected cracking in reinforced concrete bent caps at outside column locations during service load conditions. Sixteen full-scale bent cap specimens were constructed and tested under quasistatic monotonic loading. The following bent cap parameters were evaluated with regard to their influence on cracking: longitudinal reinforcement stress, size, and spacing; embedment of longitudinal reinforcement near the discontinuous end of the cap; transverse reinforcement detailing and shear strength; critical section for flexure; and side face reinforcement. Cracks were measured and reinforcement strain data were recorded throughout the load history. The experimental program confirmed that flexural crack widths during service loading are directly proportional to the level of stress in the longitudinal reinforcement and that the allowable service stress limit should be lowered to reduce such cracking. In addition, increasing the shear strength of the bent cap led to reduced inclined flexure-shear crack widths.